LOCTITE ECI7004HR

Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

LOCTITE ECI 7004HR E&C

Main features

  • High Resistivity
  • Screen Printable
  • Flexible low temperature drying cycles

Product Description

LOCTITE ECI 7004HR E&C is a screen printable, high resistance carbon solvent-based ink. It is specifically designed to allow for blending with NCI 7002 E&C to obtain the required resistance. The blended material will provide sheet resistance adjustments required in the manufacture of force sensors with slow responsive sensitivity profiles. With a maximum operating temperature of 105ºC and a heat drying cure mechanism, this ink exhibits robust performance even under challenging conditions.

LOCTITE ECI 7004HR E&C is often used to create printed resistors, including froce sensing resistor (FSR) elements, on polyester foil. With the LOCTITE NCI 7002 E&C the resistance values can be adjusted in the range of 5000 till 500.000 ohm/ sq /25 um.

LOCTITE ECI 7004HR E&C finds optimal compatibility with key substrates such as treated polyester and polyimide, ensuring consistent and reliable performance across a spectrum of assembly applications. Moreover, this ink is specially engineered to facilitate blending with LOCTITE NCI 7002 E&C, allowing for sheet resistance adjustments essential for the manufacture of force sensors with slow responsive sensitivity profiles. Additionally, LOCTITE ECI 7004HR E&C is recommended for use in the assembly of printed temperature sensors, further underscoring its versatility and adaptability in addressing diverse industry needs.

 

 

 

Product Family

LOCTITE ECI7004HR

1. Select Package Type

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 25 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
black
Density (g)
1.1 g/cm3
Solids
22.8 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
10000 mPa.s

Additional Information

LOCTITE ECI 7004HR E&C mixed with LOCTITE NCI 7002 E&C can be dried using forced air or infrared systems. Higher temperatures for longer time exposure will improve the performance. Care should be taken with infrared. Too much energy can destroy the coating. Design drying rates for the maximum the substrate and production speeds can tolerate.

The above drying profile is a guideline recommendation. Conditions (time and temperature) may vary based on customers' experience and their application requirements, as well as customer drying equipment, oven loading and actual oven temperatures.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers