PIT1S-B | 1-mil Black Polyimide (Kapton) tape with Silicone Adhesive

Main features

  • 1 mil polyimide Film
  • Opaque black color through the film
  • 3000V Breakdown Voltage

Product Description

LINQTAPE PIT1S-B is a Kapton HN Alternative whose high performance, flexible, high-temperature resistant polyimide film is used for many high-temperature applications. Polyimide is preferred over polyester for many high-temperature applications. These applications include but are not limited to semiconductor, smartcard, electronic, automotive, and general manufacturing industries.

LINQTAPE PIT1S-B Tape provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. Tapes are typically only limited by their adhesive. This Silicone tape can be used in applications up to 260°C. This PIT1S-B(lack) film has an opaque black coloring, which results in almost no light transmission, higher heat resistance and higher resistivity than the standard PIT1S.

Product Family

601805

25.4mm (1") wide x 33m (36yd) long
1. Select Width
2. Select Length

Loading pricing…

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Unit of measure Roll
Net weight 0.1 kg
Gross weight 0.1 kg
Dimensions 10 x 10 x 3 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
A layer that is applied to one surface or both to bind items together and resist their separation
Silicone
Color
The color
Black
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
25.4 µm
Thermal Properties
Temperature Resistance
Temperature resistance is the maximum temperature that the material or product can withstand for a period of time. The temperatures listed should be considered as guidelines for an operating temperature of about 30 minutes. Typically, the material can withstand much longer times at temperatures about 20°C lower and can withstand much higher temperatures for short, intermittent times.
260 ˚C
Electrical Properties
Breakdown Voltage
Breakdown voltage is the minimum voltage necessary to force an insulator to conduct some amount of electricity. It is the point at which a material ceases to be an insulator and becomes a resistor that  conducts electricity at some proportion of the total current.  After dielectric breakdown, the material may or may not behave as an insulator any more because of the molecular structure alteration. The current flow tend to create a localised puncture that totally alters the dielectric properties of the material. This electrical property is thickness dependent and is the maximum amount of voltage that a dielectric material can withstand before breaking down. The breakdown voltage is calculated by multiplying the dielectric strength of the material times the thickness of the film.
3000 V
Other Properties
RoHS Compliant
RoHS is a product level compliance based on a European Union Directive which restricts the Use of certain Hazardous Substances in Electrical and Electronic Equipment (RoHS). Products compliant with this directive do not exceed the allowable amounts of the following restricted materials: lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls (PBB) and polybrominated diphenyl ethers (PBDE), with some limited exemptions
Yes
Mechanical Properties
Adhesion Strength
Adhesion is the bond strength measurement of a coating to a substrate. When an adhesive is bonded to an item or surface, numerous physical, mechanical and chemical forces come into play, which may have an effect on each other.
25 Oz/in
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
55 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
338 N/cm