LINQ PIT1S

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

Polyimide Tape Build PIT1S | 1-mil Polyimide (Kapton) Tape with Silicone Adhesive PIT1S | 1-mil Polyimide (Kapton) Tape with Silicone Adhesive PIT1S | 1-mil Polyimide (Kapton) Tape with Silicone Adhesive PIT1S | 1-mil Polyimide (Kapton) Tape with Silicone Adhesive 1-mil Polyimide Tape Silicone Adhesive Single-Sided 510mm Roll of LINQTAPE

Main features

  • 1 mil polyimide film
  • Silicone adhesive
  • >6000V breakdown voltage

Product Description

LINQTAPE™ PIT1S-Series is a high-temperature resistant polyimide tape designed for both permanent and temporary bonding in many high temperature applications. These applications can be found in semiconductor, smartcard, electronic, automotive and general manufacturing industries. It is a good alternative product to Nitto Permacel P-221, 3M 5413 and Intertape 4428. 

Key Features:

  • Superior electrical insulation - Insulation Temperature Rating Class H (180°C) 
  • Superior heat resistance - Operation temperature up to 260°C
  • Good puncture, tear and abrasion resistance 
  • High-temperature resistant and solvent-against silicone adhesive 

Typical Applications: PCB solder masking,  electrical insulation used in coils/motors/transformers/bobins/capacitors, etc.

LINQTAPE™ PIT1S-Series Tape comes in 33 meter (36 yard) rolls of varying widths. LINQTAPE PIT-S polyimide films with silicone adhesive are available in a range of thicknesses, starting from 0.5 mil (12.7µm) thickness and up. Custom thicknesses are available upon request.

 

Product Family

LINQ PIT1S

1. Select Width
2. Select Length

Loading pricing…

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
A layer that is applied to one surface or both to bind items together and resist their separation
Silicone
Adhesive Thickness
Adhesive thickness indicates the thickness of an adhesive layer. It refers to the adhesive thickness of a single side so for double sided tapes it always needs to be multiplied.
38.1 µm
Chemistry Type
Polyimide
Color
The color
Amber
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
25.4 µm
Release Liner
A paper or plastic-based film sheet used to prevent a sticky surface from prematurely adhering
None
Single or Double-Sided Adhesive
Describes whether a tape is single- or double-sided. If it is single-sided, it has adhesive only on one side of the backing film. If it is double-sided, then it has adhesive on both sides of the backing film.
Single-Sided
Special Layer
None
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
63.5 μm
Thermal Properties
Temperature Resistance
Temperature resistance is the maximum temperature that the material or product can withstand for a period of time. The temperatures listed should be considered as guidelines for an operating temperature of about 30 minutes. Typically, the material can withstand much longer times at temperatures about 20°C lower and can withstand much higher temperatures for short, intermittent times.
260 ˚C
Electrical Properties
Breakdown Voltage
Breakdown voltage is the minimum voltage necessary to force an insulator to conduct some amount of electricity. It is the point at which a material ceases to be an insulator and becomes a resistor that  conducts electricity at some proportion of the total current.  After dielectric breakdown, the material may or may not behave as an insulator any more because of the molecular structure alteration. The current flow tend to create a localised puncture that totally alters the dielectric properties of the material. This electrical property is thickness dependent and is the maximum amount of voltage that a dielectric material can withstand before breaking down. The breakdown voltage is calculated by multiplying the dielectric strength of the material times the thickness of the film.
>6000 V
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
236 kV/mm
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
10000000000000 Ohms⋅cm
Other Properties
RoHS Compliant
RoHS is a product level compliance based on a European Union Directive which restricts the Use of certain Hazardous Substances in Electrical and Electronic Equipment (RoHS). Products compliant with this directive do not exceed the allowable amounts of the following restricted materials: lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls (PBB) and polybrominated diphenyl ethers (PBDE), with some limited exemptions
Yes
VOC-Free (100% solids content)
VOC means Volatile Organic compound. VOCs are evaporating molecules and are literally everywhere around us. Our scents are volatile organic compounds, most of the things that we smell are VOC etc. So what do we mean when we state that a product is VOC free? A VOC free product, according to the FTC is one where: 1)VOCs have not been intentionally added to the product. 2)The presence of VOCs at that level does not cause material harm that consumers typically associate with VOCs, including but not limited to, harm to the environment or human health. 3)The presence of VOCs at that level does not result in concentrations higher than would be found at background levels in the ambient air.
Yes
Mechanical Properties
Adhesion Strength
Adhesion is the bond strength measurement of a coating to a substrate. When an adhesive is bonded to an item or surface, numerous physical, mechanical and chemical forces come into play, which may have an effect on each other.
26 Oz/in
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
55 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
89 N/cm

Additional Information

  Typical Applications

 

Comparing with Kapton tape with acrylic adhesive (PIT1A series), silicone adhesives tape can withstand higher temperature range as compared to acrylic adhesives, which provide a wider appilication range. Acrylics have the property of being more brittle and as such they can crack at extremely low temperatures too. Generally speaking, the acrylic adhesive will have higher adhesion at mid-range temperatures (0°C to 100°C), but silicone adhesives have higher adhesion at lower temperatures (under 0°C) and higher temperatures (above 100°C). PIT1S-Series are suitable for continous cold and high temperature environments, typical applications are:

  • Masking against chemicals, heat and other hash conditions
  • PCB masking for wave solder and solder reflow process
  • Protective layer, ground, barrier and cross over insulation for electrical components like bobbin, toroidal coils, etc.
  • End-turn bunding and connection insulation for small motors, etc.

 

 

  Replacement Suggestion

Popular Brand Names Krayden LINQTAPE Part # Product Description

Dupont Kapton Tapes

LINQTAPE PIT1N-Series

1 mil HN Polyimide Film | No Adhesive

Nitto Permacel P-224

3M 1206

LINQTAPE PIT1A-Series

1-mil Single-sided Polyimide (Kapton) Tape With Acrylic-based Adhesive

Nitto Permacel P-221

3M 5413

Saint-Gobain Furon K250

Intertape 4428

LINQTAPE PIT1S-Series 1-mil Single-sided Polyimide (Kapton) Tape With Silicone-based Adhesive
Nitto Permacel P-223 LINQTAPE PIT1SD-Series 1-mil Double-sided Polyimide (Kapton) Tape With Silicone-based Adhesive

Nitto Permacel P-222

Saint-Gobain Furon K350

Intertape 4429

LINQTAPE PIT2S-Series 2-mil Single-sided Polyimide (Kapton) Tape With Silicone-based Adhesive
Saint-Gobain Furon K104 LINQTAPE PIT5S-Series 5-mil Single-sided Polyimide (Kapton) Tape With Silicone-based Adhesive

 

 

 

 

 

{tab=Pricing & Availability}

Pricing for {product_name}

Volume Price Breaks can be seen for each product by clicking on its respective link under the DESCRIPTION column and looking to the volume price break table to the right of the product image. Price per unit is reflected in this table and used during checkout.

KRAYDEN lists all its prices without taxes, shipping payment charges or discounts. KRAYDEN has entities in Canada and the Netherlands, and if your shipping address is one of these two countries, applicable taxes will be applied.

If your shipping address is to the United States, we request your company?s Employer Identification Number (EIN) or Tax Identification Number (TIN). This is a unique 9-digit number assigned by the IRS and is required for all cross-border shipments. Failure to provide this number could result in delays to your order.

If your shipping address is within the EU, but outside the Netherlands, then we are required to request your company's Value Added Tax (VAT, BTW, MwSt) number to be able to ship the goods tax-free. For all other countries, no taxes are levied on your orders.

DON'T LIKE THESE PRICES? Tell us what you will pay for what order quantity.


Shipping Charges for {product_name}

All prices shown are ex-works KRAYDEN, but during the checkout process, you will be given several shipping options including Canada Post, TNT, UPS or the choice of using your own freight forwarder. Depending on your shipping address, the shipping charges will be calculated as follows:

  • Europe, Middle East, Asia and Africa: Shipping from KRAYDEN Netherlands (Amsterdam)
  • Canada, USA, Mexico and South America: Shipping from KRAYDEN Canada (Ottawa)

Payment option for {product_name}

During the checkout process, you will be presented with several payment options including:

  • Credit Card (We accept VISA and Mastercard)
  • Bank Transfer (You will be given the payment instructions at the time of order placement)
  • PayPal (Where you can also pay with American Express Cards)
  • Purchase Order (You must be preapproved first. See our Online Credit Application)

Availability for {product_name}

To the right of the product is a small icon that lets you know the availability and leadtime of the product. This leadtime is the time to ship the product and delivery times vary based on the method of delivery you select at the time you place your order.

Contact us if anything is unclear or you need more assistance.

{tab=Competitive Crossovers}

Compare price and quality of LINQTAPE to DuPont, 3M, Furon, Nittto & these other brands
Popular Brand1
Names
Product
Description
KRAYDEN LINQTAPE
Part#
  • Nitto Permacel P-224
  • DuPont Kapton Tape
  • 3M 1206
1-mil Single-Sided Polyimide (Kapton) Tape with Acrylic-based Adhesive
  • LINQTAPE PIT1A-Series
    ie. LINQTAPE PIT1A/25.4
  • Nitto Permacel P-221
  • DuPont Kapton Tape
  • 3M 5413
  • Saint-Gobain Furon® K250
  • Intertape 4428
1-mil Single-Sided Polyimide (Kapton) Tape with Silicone-based Adhesive
  • LINQTAPE PIT1S-Series
    ie. LINQTAPE PIT1S/25.4
  • Nitto Permacel P-222
  • DuPont Kapton Tape
  • Saint-Gobain Furon® K350
  • Intertape 4429
2-mil Single-Sided Polyimide (Kapton) Tape with Silicone-based Adhesive
  • LINQTAPE PIT2S-Series
    ie. LINQTAPE PIT2S/25.4
  • DuPont Kapton Tape
  • Saint-Gobain Furon® K104
5-mil Single-Sided Polyimide (Kapton) Tape with Silicone-based Adhesive
  • LINQTAPE PIT5S-Series
    ie. LINQTAPE PIT5S/25.4
  • Nitto Permacel P-223
  • DuPont Kapton Tape
1-mil Double-Sided Polyimide (Kapton) Tape with Silicone-based Adhesive
  • LINQTAPE PIT1SD-Series
    ie. LINQTAPE PIT1SD/25.4
NittoPermacel
3M1206Saint-GobainFuronIntertape
1 Permacel® Kapton®, 3M®, Furon® and Intertape are registered trademarks of Nitto, DuPont, 3M, Saint-Gobain and Intertape respectively and are not affiliated with this site.
 

{tab=Videos & Other Media}

Videos & Other Related Media

Sorry, there are no related videos for {product_name} at this time.

{tab=Product Reviews}

Product Reviews for {product_name}

{review}

{tab=View Blogs & Forum}

Read and discuss {product_name} on KRAYDEN's Blog and Forum

KRAYDEN is different. Unlike other business to business enterprises, we encourage our customers to discuss, critique, and otherwise comment on the products we offer. Get more technical information, read detailed posts, and see what customers have to say about about {product_name} on our Corporate Blog and Forum.

  • Read more about {product_name} on our Blog.
  • Join the discussion about {product_name} on our Forum.

{/tabs}

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers