DOWSIL TC-5622

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

DOWSIL TC-5622 THERMALLY CONDUCTIVE COMPOUND

Main features

  • 4.3 W/(m K) Thermal Conductivity
  • 0.06 deg C cm^2/W Thermal Resistance
  • Non-Curing, Solventless Compound for Dispensing or Printing

Product Description

DOWSIL™ TC-5622 Thermally Conductive Compound is a grey, flowable, non-curing silicone thermal interface compound for transferring heat from electronic devices and PCB assemblies to heat sinks or chassis surfaces. The solventless, filled polydimethylsiloxane formulation has a typical thermal conductivity of 4.3 W/m·K and can achieve a thin 0.02 mm bondline. At a reported pressure of 25 N/cm², its typical area-normalised thermal resistance is 0.06 °C·cm²/W. The material can be dispensed, stencil printed, or screen printed and remains non-curing, supporting straightforward application and rework in computer MPU, power-module, and other electronics cooling interfaces.

Key Features

  • Non-curing, solventless silicone thermal compound
  • Typical thermal conductivity of 4.3 W/m·K
  • Typical thermal resistance of 0.06 °C·cm²/W at 25 N/cm²
  • Typical 0.02 mm bondline thickness under the reported test condition
  • Flowable 95,000 cP consistency for dispense, stencil-print, or screen-print application
  • Grey grease-like form with low bleed and high-temperature stability positioning
  • Reworkable thermal interface for modules, PCB assemblies, heat sinks, and chassis

Suitable for

  • Computer MPU-to-heat-sink interfaces
  • Power-module cooling interfaces
  • PCB assembly-to-heat-sink or chassis interfaces
  • Dispensed, stencil-printed, and screen-printed thermal interface processes

Technical Specifications

Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
95000 mPa.s
General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
2.5
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
4.3 W/m.K
Thermal Impedance
0.06 °C·cm²/W

Additional Information

Non-curing thermal interface compound

DOWSIL™ TC-5622 Thermally Conductive Compound

A grey, flowable, non-curing silicone compound that fills microscopic surface irregularities between electronic devices or PCB assemblies and heat sinks or chassis surfaces. Its 4.3 W/m·K typical thermal conductivity, low reported thermal resistance, and ability to form a thin bondline support efficient interface heat transfer while retaining a reworkable grease-like form.

Non-curing silicone 4.3 W/m·K 0.02 mm bondline Solventless formulation Dispense or print
DOWSIL TC-5622 Thermally Conductive Compound product packaging

DOWSIL TC-5622 Thermally Conductive Compound product packaging

As supplied

Material form and physical properties

TC-5622 is a filled polydimethylsiloxane compound supplied as a grey, grease-like, non-curing material. The values below are typical and are not sales specifications.

Property Typical value / characteristic Selection relevance
Physical form Grey grease-like compound Non-curing interface material intended to remain in a grease state after installation.
Composition Filled polydimethylsiloxane Silicone matrix with heat-conductive metal-oxide fillers.
Viscosity 95,000 cP (95 Pa·s) Supports dispense, stencil-print, and screen-print process evaluation.
Specific gravity 2.5 typical Useful for estimating applied mass from material volume.
SDS relative density 2.55 typical The SDS reports a closely aligned relative density; treat this as a context-dependent source difference rather than a specification conflict.
Application and installation

Apply a controlled, thin thermal interface

Apply TC-5622 by dispensing, stencil printing, or screen printing to create a continuous interface between the heat source and heat sink or chassis. Assemble the mating surfaces with controlled pressure and material quantity so the compound fills surface irregularities without an unnecessarily thick layer. Because the material does not cure, installed retention depends on the mechanical assembly and interface design.

  • Clean and prepare the mating surfaces using an assembly-specific procedure.
  • Control the printed or dispensed quantity to target the required bondline and coverage.
  • Avoid routine solvent exposure; only minimal or intermittent solvent exposure is described as generally resistant.
  • Validate squeeze-out, migration, bleed, pump-out, rework, and thermal performance in the intended assembly.
Illustration of dispensing or printing DOWSIL TC-5622 between an electronic device and heat sink

Dispensing or printing DOWSIL TC-5622 between an electronic device and heat sink

Dispense

Apply metered dots, beads, or patterns where automated placement and part-specific coverage are required.

Stencil print

Use a controlled stencil to deposit repeatable shapes and material volume across multiple interface locations.

Screen print

Suitable for patterned application where the equipment, mesh, print settings, and transfer efficiency are validated for the material.

Storage and handling

Store TC-5622 in its original, properly labelled packaging with the cover tightly attached to limit contamination. Follow any special storage instructions and the expiry date shown on the product label. Before handling, review the current regional safety documentation and container label. Use adequate ventilation and suitable workplace controls based on the applicable risk assessment.

Installed thermal performance

Bulk conductivity and pressure-dependent interface data

Thermal conductivity describes the bulk compound, while the reported thermal resistance is tied to the stated pressure and bondline. Installed performance also depends on surface finish, interface area, assembly pressure, material coverage, orientation, and operating conditions.

Property Typical value Required context
Thermal conductivity 4.3 W/m·K Bulk-material property; it does not independently establish total interface or system resistance.
Area-normalised thermal resistance 0.06 °C·cm²/W Reported at 25 N/cm²; preserve pressure and bondline when comparing materials.
Bondline thickness 0.0008 in (0.02 mm) Reported with the associated thermal-resistance condition; not a universal installed thickness.

Do not compare the 4.3 W/m·K conductivity or 0.06 °C·cm²/W resistance directly with another TIM unless the test method, bondline, pressure, temperature, and interface configuration are sufficiently aligned.

Applications

Thin, reworkable thermal interfaces for electronics cooling

TC-5622 is designed for cooling modules, including computer MPUs and power modules. Application suitability depends on interface pressure, gap, surface condition, mechanical retention, orientation, electrical requirements, and the operating environment.

Computer MPU mounted to a heat sink with a thin thermal compound layer

Computer MPU cooling

Designed for module interfaces where a processor or similar heat source is mechanically clamped to a heat sink through a thin compound layer.

Power module attached to a heat sink through a printed thermal compound interface

Power modules

Suitable for evaluation between power modules and heat sinks or chassis surfaces when the assembly provides controlled pressure and mechanical retention.

PCB system assembly thermally coupled to a chassis using dispensed compound

PCB assembly-to-chassis interfaces

May be considered where a PCB system assembly or mounted component transfers heat to a heat sink, spreader, housing, or chassis through a thin reworkable layer.

 

Evaluate TC-5622 for your thin thermal interface

Krayden can help review interface pressure, target bondline, surface condition, dispensing or printing method, material coverage, mechanical retention, rework requirements, and assembly-level thermal validation for DOWSIL™ TC-5622.

Contact Krayden Technical Support

Leading Brands Trust in Our Products and Services