PEAM-645 High Tg Polyester Acrylate/Methacrylate

Harmonization Code : 3906909090 | Acrylic polymers in primary form Others>Others

PEAM-645 High Tg Polyester Acrylate/Methacrylate

Main features

  • High Tg
  • Low CTE
  • High adhesion to various substrates

Product Description

PEAM-645 is a polyester acrylate/methacrylate that exhibits low CTE, high Tg, and high modulus. The oligomer has very high thermal stability and low volatility. It can be used as a base resin in a formulation or as an additive. It exhibits good adhesion on various substrates. The oligomer also exhibits good hydrolytic stability

PEAM-645 is recommended for use as a base resin in adhesive applications or coating applications. The material if used alone can exhibit brittleness and the incorporation of a toughener (such as ABS, or hyperbranched polyester) is recommended. The oligomer has good solubility in both aliphatic and aromatic co-monomers. PEAM-645 is more akin to epoxies with the smaller molecular weight (still big compared to most epoxies but much smaller than the PEAM-1044) and with higher Tg as a result. It common to mix these product for optimal results.

Product Family

233259

1kg jar
1. Select Package Type

Loading pricing…

Product availability
US No longer available
CA No longer available
EU Shipping in 2 weeks
Packaging
Unit of measure Jar
Net weight 1 kg
Gross weight 1.3 kg
Dimensions 10 x 10 x 20 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Amber Liquid
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
160 °C
Weight Loss @ 300°C
3 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
5,000 mPa.s