LOCTITE ABLESTIK QMI550

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE ABLESTIK QMI550

Main features

  • Non conductive
  • Hydrophobic
  • Skip Cure

Product Description

LOCTITE ABLESTIK QMI550 non conductive die attach paste was designed to attach integrated circuits and components to advanced substrates. It is an off white, fluoropolymer filled, BMI hybrid that is stable at high temperatures.

LOCTITE ABLESTIK QMI550 has excellent interfacial adhesion strength and cohesive strength with great dielectric properties. It is designed for PBGA, CSP, array packages and die stacking substrates and works great with Solder masks, BT, FR, Polyimide, Au and other organic surfaces. Due to its higher modulus and soft PTFE filler, it can be used for small 1x1 die, specifically for small die stacking and sensor die attach.

Skip Cure

  • ≥10 seconds @ 150°C
Product Family

233562

5cc in10cc Syringe - 1767157
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 35 days
Packaging
Unit of measure Syringe
Net weight 7 g
Gross weight 16.6 g
Dimensions 3 x 1.7 x 8.9 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
24 hours
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.32
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
-10 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.3 W/m.K
Chemical Properties
Moisture absorption
0.29 %
Physical Properties
Thixotropic index
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten. A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads. It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
6.4
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
11,500 mPa.s

Leading Brands Trust in Our Products and Services