ABLESTIK 789-3

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE ABLESTIK 789-3

Main features

  • Non conductive
  • Good moisture resistance
  • Substrate attach

Product Description

LOCTITE ABLESTIK 789-3 die attach adhesive is designed for microelectronic applications. This adhesive exhibits strong adhesion to difficult-to-bond metals and retains its bond strength after exposure to moisture.

LOCTITE ABLESTIK 789-3 is a non conductive epoxy adhesive with good moisture resistance and high bond strength. It is typically used for substrate attach and package sealing on gold, silver and copper substrates.

Cure Schedule

  • 30 minutes @ 150°C 
  • 4 hours @ 93°C
Product Family

ABLESTIK 789-3

1. Select Package Type

Loading pricing…

Product availability
US Shipping in 20 days
CA Shipping in 12 weeks
EU Shipping in 40 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
2184 hours
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
126 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.3 W/m.K
Weight Loss @ 300°C
0.28 %
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
2000000000000000 Ohms⋅cm
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
36,500 mPa.s